I still need to get some optical quality MgF2 and whatever other materials are needed for the enhanced coating. I do have pure aluminum. I have not been able to find much in the way of what recipe is used for the enhanced coating, though.
-
Oh, I also need to figure out my tooling factor for coating thickness. I am going to coat some samples this week and then take them down to PSU where I have a friend with a AFM to measure the thickness.